Foundry Metallurgy - Study Mode
[#46] Sprue in casting refers to . . . . . . . .
Correct Answer
(D) Vertical passage
[#47] The shrinkage allowance for 6mm section malleable cast iron is . . . . . . . . mm.
Correct Answer
(A) 10.4
[#48] If two parts of a mould are not joined properly, the casting may have the following defect.
Correct Answer
(D) Flash
[#49] The solidification time for a cube casting having 5 cms side is 10 minutes. Under similar condition of heat transfer, the solidification time, inminutes, for a cube casting having 10 cm side will be
Correct Answer
(C) 40
[#50] In a casting, shrinkage occurs
Correct Answer
(B) only during transformation from liquid to solid